Electrodes
 
 
MIG/TIG
 
 
Hardfacing
 
 
Solders
 
 
 

77 Information

Available in 1/8"


Tensile (as welded): 52,500 - 55,000 PSI
Tensile (slightly worked): 56,100 - 58,250 PSI
Elongation (in red zone): 71%
Elongation (in weld room temp. 70): 59%
Yield (as welded): 44,550 PSI
Yield (slightly worked): 45,750 PSI
Color match (Grey Iron): Good
Machinability: Excellent
Weld Appearance: Excellent
Weldability: Excellent

Cross Strength (Build up area)*Points
(In total Sq. Ins. Area)Thickness100 Index
8 sq. ins.1/4"90
16 sq ins.3/8"88
32 sq ins.1/2"87
64 sq ins.1-1/2"84



How to Apply

Begin by beveling the joint. Drill holes 1/2" from each end of the crack to prevent further cracking while welding. Tack weld to retain alignment. Use AC or DC with reverse polarity. (60-110 amps for 1/8" rods, 90-140 amps for 5/32" rods) Maintain a short to medium arc and make short passes and peen each pass promptly to chip off slag before cooling. Continue back whipping and overlapping until all deposits are connected. Cool naturally.




   

 